This is an open access article distributed under the Creative Commons Attribution License which permits unrestricted use, distribution, and reproduction in any medium, provided the original work is properly cited.
University of Zenica, Faculty of Metallurgy and Technology Travnička cesta 1, Zenica, University of Zenica , Zenica , Bosnia and Herzegovina
Faculty of Metallurgy and Technology Travnička cesta 1, Zenica, University of Zenica , Zenica , Bosnia and Herzegovina
Faculty of Metallurgy and Technology Travnička cesta 1, Zenica, University of Zenica , Zenica , Bosnia and Herzegovina
This paper describes a few examples of the recovery of manganese from steel slag and dust by using different technologies based on acid leaching.
Reductive leaching in sulfuric acid (H2SO4) for recovery of manganese from electric arc furnace dust (EAFD) was represented. Recovery of manganese and iron was increased with increasing in the sulfuric acid concentration. By using different reductantcs such as oxalic acid and hydrogen peroxide were revealed a higher manganese recovery than the other reductants. The results were showed that leaching of manganese was accomplished at 0.31 mol/L oxalic acid concentration, 2 mol/L H2SO4, a liquid/solid ratio of 30/1 at 70 °C and with 90 min leaching time.